    水泥自流平施工過(guò)程注意事項(xiàng)
    1、環(huán)境施工溫度,以15-25℃為宜.
    2、基層應(yīng)滿足:C20以上,無(wú)起砂、空鼓、起殼、油脂、裂紋等缺陷.
    基層含水率不大于6%.
    3、施工場(chǎng)所門窗可以封閉,施工過(guò)程沒(méi)有穿堂風(fēng),無(wú)陽(yáng)光直射.
    4、界面劑完全干燥后再進(jìn)行自流平施工.
    5、水泥自流平必須用機(jī)械攪拌.
    英語(yǔ)人氣:430 ℃時(shí)間:2020-05-13 01:26:51
    優(yōu)質(zhì)解答
    Cement self-leveling construction process the matters needing attention
    1,environment construction temperature to 15-25 ℃ advisable.
    2,the basic unit should meet:C20 above,no rise sand,empty drum,the shell,grease,crack defects,etc.
    The moisture content is not more than 6%.
    Three,the construction site doors and Windows can be closed,construction process does not drafts,no direct sunlight.
    4,interface agent completely dry again self-leveling construction.
    5,cement self-leveling must use mechanical agitation.